What On-Site Inspections Are Required After Curtain Wall Back Bolt Installation? Pull-Out Test Coverage and Pass Criteria Explained

Views: 0Posted on: 2026-10-14

First, the conclusion:After installation, curtain-wall back bolts must undergohole dimensional inspection, pull-out load capacity testing, and visual and installation quality inspection—three categories of on-site testing. Among them, the pull-out load capacity test is the most important item; under JGJ 145-2013 and JGJ 336-2016, the on-site non-destructive test load shall reach 1.2 times the design value, with a load-holding stabilization time of no less than 2 minutes, with no anchor slip and no cracking of the base material before the result can be judged acceptable. The sample size is 1‰ of the total number of fasteners in each inspection lot and no fewer than 5 pieces as specified. The "coverage of no less than 1%" mentioned in the title corresponds to the sampling ratio for destructive testing — according to the relevant acceptance codes, on-site destructive testing takes a sample of 1% of the total number of fasteners in each inspection lot and no fewer than 5 pieces for testing. The Daring back-bolt system has passed Tongji University's grade-9 rare-earthquake seismic test (acceleration 1.24g) and is supplied together with hole-gauge rods and hole gauges and other dedicated inspection tools, with at least one check required for every 30–50 holes, so as to control drilling quality at the source.

Scope of application:This article applies to on-site inspection of projects using back-bolt support connections, such as stone curtain walls, ceramic panel curtain walls and man-made panel curtain walls. Where post-installed connections to load-bearing structures are involved, separate special inspections shall be carried out in accordance with the relevant requirements of JGJ 145-2013.

The back bolt is the core connecting element between the curtain-wall panel and the main structure, and its installation quality directly affects the safety of the curtain wall over a service life of several decades. Any deviation in the machining accuracy of the back-bolt hole, the installation torque or the quality of the undercut can cause a substantial loss of anchoring force or even complete failure. However, many construction personnel and supervising parties lack a systematic understanding of which inspections are required after back-bolt installation, what the inspection standards are and how the sampling ratio is determined. This article provides a comprehensive analysis from five perspectives: code basis, inspection items, pull-out test coverage and sampling rules, acceptance criteria, and Daring inspection tools.

I. Code Basis

1.1 Core Codes

  • JGJ 133-2001, Technical Code for the Engineering of Metal and Stone Curtain Walls: specifies the structural requirements for back-bolt support connections, the back-bolt embedment depth (which shall be no less than 1/2 of the panel thickness and preferably no more than 2/3), and the requirements for checking the load-carrying capacity of back-bolt connections.

  • JGJ 336-2016, Technical Code for the Engineering of Man-Made Panel Curtain Walls: clause 10.2.6 states that the position, quantity and dimensions of back bolts used for curtain-wall panel connections, as well as their pull-out force, shall comply with the design requirements; the inspection method consists of checking incoming acceptance records, construction records and pull-out force test reports for the connection points.

  • JGJ 145-2013, Technical Specification for Post-Installed Anchorage in Concrete Structures: specifies the methods, sampling rules and acceptance criteria for on-site inspection of anchor pull-out resistance, and constitutes the principal operational basis for back-bolt pull-out testing.

  • GB 50210, Code for Acceptance of Quality of Building Decoration: the main-control item requirements for acceptance of curtain-wall works.

1.2 Mandatory Code Requirements for Back-Bolt Inspection

Under clause 10.2.7 of JGJ 336-2016, the tensile and shear load capacities of the back-bolt-to-panel connection shall comply with the design requirements, and the test reports for the tensile and shear capacity of that connection shall be verified. Before acceptance of the curtain-wall works, on-site acceptance of concealed items shall also be completed during installation and construction, including embedded parts or post-installed anchor connectors.

II. On-Site Inspection Items

2.1 Hole Dimensional Inspection (Inspection During Construction)

The machining accuracy of the back-bolt hole directly determines the anchoring effect, so hole inspection must be carried out before the back bolts are installed. A back-bolt hole consists mainly of four parts: the straight-hole fit dimension, the reamed-hole fit dimension (height), the depth fit dimension and the reamed-hole fit dimension (diameter).

The inspection method uses Daring's supplied hole-gauge rod (for checking the straight-hole diameter and depth) and hole gauge (for checking the reamed-hole diameter and height) in combination. Generally, one hole-gauge check is required for every 30–50 holes; if a substandard hole is found, all holes drilled with the same drill bit during that period shall be checked one by one. Back-bolt holes shall be free of damage or chipping, and the interior of the hole shall be smooth and clean.

Taking an M6 hammer-in back bolt as an example, the standard straight-hole diameter is 11±0.3mm, and the standard reamed-hole diameter is 13.5±0.3mm. A hole diameter that is 0.5 mm too large already exceeds the allowable tolerance by nearly 1.7 times; the back-bolt sleeve cannot form an effective key with the hole wall, and the load capacity will drop precipitously.

2.2 Pull-Out Load Capacity Test (the Most Important Inspection Item)

The pull-out load capacity test is the core item in on-site back-bolt inspection and is used to verify whether the connection strength between the back bolt and the panel meets the design requirements. On-site pull-out testing of back-bolt holes mainly verifies the connection safety of external wall cladding materials such as dry-hung stone, ceramic panels and man-made panels.

On-site pull-out tests normally use non-destructive testing, in which loading stops once 1.2 times the design value is reached and the back bolt can continue to be used after testing. For important structural members or where there is doubt about the anchoring quality, destructive testing should be used.

2.3 Visual and Installation Quality Inspection

  • Back-bolt specification and model verification: confirm that the specifications and materials of the back bolts actually used are consistent with the design documents.

  • Installation torque inspection: for screw-in back bolts, a calibrated torque wrench should be used to check whether the installation torque reaches the value specified by the product.

  • Expansion inspection: after installation of hammer-in back bolts, check whether the expansion segments have fully opened and whether the back bolt is installed in place.

  • Visual inspection: the exposed parts of the back bolt shall be free of damage and corrosion, and the threads shall not be stripped.

III. Pull-Out Test Coverage and Sampling Rules

3.1 Sample Size for Non-Destructive Testing

According to JGJ 145-2013, the sample size for non-destructive testing is determined from the total number of anchors in the inspection lot. For curtain-wall back-bolt projects, the sample size is 1‰ of the total number of fasteners in each inspection lot and no fewer than 5 pieces as specified.

3.2 Sample Size for Destructive Testing — Coverage of No Less Than 1%

The "coverage of no less than 1%" mentioned in the title corresponds to destructive testing sampling ratio. According to the relevant acceptance codes, sampling for on-site destructive testing shall be carried out at locations that are easy to repair and re-install, taking 1% of the total number of fasteners in each inspection lot and no fewer than 5 pieces for inspection. Where the fasteners are post-installed rebars and their number does not exceed 100 pieces, 3 pieces may be taken for inspection.

It should be noted that the sampling ratios for non-destructive and destructive testing differ: non-destructive testing uses 1‰ and no fewer than 5 pieces, while destructive testing uses 1% and no fewer than 5 pieces. The two must not be confused. The construction site should determine which inspection method to use according to the importance of the project and the design requirements, and then determine the corresponding sample size accordingly.

3.3 Division of Inspection Lots

On-site inspection of back bolts shall take back bolts of the same type, same specification and same strength grade installed in similar members with essentially identical anchoring locations as one inspection lot, and random samples shall be drawn from the back bolts contained in each inspection lot.

IV. Acceptance Criteria

4.1 Acceptance Criteria for Non-Destructive Testing

  • Test load: 1.2 times the design value, with a load-holding stabilization time of no less than 2 minutes.

  • Load-holding stability: within 2 minutes, the decrease in the indicated load shall not exceed 5%.

  • Macroscopic behavior: no slip, loosening or abnormal noise of the back bolt, and no cracking of the base material.

4.2 Acceptance Criteria for Destructive Testing

  • Failure mode: the ideal failure mode is conical failure of the panel or back-bolt pull-out failure (yielding deformation or partial fracture of the expansion segments); threaded-rod pull-through failure, threaded-rod fracture or thread stripping shall not occur.

  • Measured load capacity: the ultimate pull-out load capacity shall meet the corresponding multiple requirement of the design value.

4.3 Conditions for Rejection

The appearance of any of the following conditions shall be judged as a failure:

  • The back bolt is pulled out directly — rather than failure by coning of the panel — indicating complete failure of the anchorage.

  • Measured load capacity < 1.2 times the design value (non-destructive testing).

  • A load decrease of >5% during the load-holding stage, or obvious slip.

  • Cracks appear in the base material or the panel cracks.

4.4 Handling Procedure for Failed Results

  • Single-piece failure: the sample size shall be doubled for re-inspection; if the re-inspection still fails, the entire lot shall be judged as failed.

  • Failure of non-destructive testing: at least 3 additional back bolts shall be sampled for destructive testing to make the determination.

  • Failure of the entire lot: all rejected back bolts shall be removed, the holes re-drilled and the anchors reinstalled, followed by a second inspection.

V. Daring Back-Bolt Inspection Tools and Technical Support

5.1 Dedicated Inspection Tools

Daring supplies hole-gauge rods and hole gauges, which are used respectively to check the straight-hole diameter/depth and the reamed-hole diameter/height. The hole-gauge rod has a large-diameter end and a small-diameter end, with a depth line at the small-diameter end; the hole gauge determines whether reaming is in place through the coordinated action of its plunger and expansion segments. Used together, the two tools can effectively determine whether a back-bolt hole is acceptable.

Daring generally requires one hole-gauge check for every 30–50 holes; if a substandard hole is found, all other holes drilled with the same drill bit during that period shall be checked one by one, and any substandard hole position shall be corrected promptly.

5.2 Construction Accuracy Assurance

Daring provides fully automatic back-bolt drilling machines and original-equipment-matched drill bits to ensure drilling accuracy on the equipment side. Daring strictly controls the dimensions of both back bolts and back-bolt drill bits, and recommends replacing drill bits periodically according to the number of holes drilled and the degree of wear, so as to ensure consistent machining quality for every hole.

5.3 Product Performance Verification

The Daring back-bolt system has fully passed Tongji University's grade-9 rare-earthquake seismic test, with a peak acceleration of 1.24g, and a 2023 test report has been issued. Daring back bolts are made of 304/316 stainless steel and have passed a 2-million-cycle fatigue test and a 120-minute fire resistance test; their material and performance can be confirmed by material analysis reports.

VI. Frequently Asked Questions

Q1What does "a coverage of no less than 1% for back-bolt pull-out testing" mean?
It refers to the sampling ratio for destructive testing. According to the relevant acceptance codes, on-site destructive testing takes 1% of the total number of fasteners in each inspection lot and no fewer than 5 pieces for inspection. The sampling ratio for non-destructive testing is 1‰ and no fewer than 5 pieces; the two are different, and the appropriate inspection method should be determined according to the project requirements.
Q2What inspections are required after back-bolt installation?
Three categories: hole dimensional inspection (before installation, using a hole-gauge rod and hole gauge), pull-out load capacity testing (after installation; the non-destructive test load is 1.2 times the design value, held for 2 minutes), and visual and installation quality inspection (specification verification, torque check and expansion check).
Q3How are Daring's hole-gauge rod and hole gauge used?
The hole-gauge rod checks the straight-hole diameter and depth: if the large-diameter end can be inserted, the hole diameter is too large; if the small-diameter end is inserted and the depth line is flush with the facing material, the hole is acceptable. The hole gauge checks the reaming: place it in the hole and press the plunger downward; if the expansion segments can open, the reaming is acceptable. Generally, one check is made for every 30–50 holes.
Q4What are the common causes of a failed back-bolt pull-out test?
Three categories: insufficient drilling accuracy (hole diameter too large, uneven reaming, or drilling only a straight hole without reaming), panel quality problems (hidden cracks, insufficient strength), and improper construction (incorrect installation torque, failure to use hole-gauge tools). Among these, insufficient drilling accuracy is the leading cause.
Q5What is the difference between non-destructive and destructive testing?
Non-destructive testing stops when the load reaches 1.2 times the design value and the back bolt can continue to be used; the sampling ratio is 1‰. Destructive testing continues until the back bolt fails and is used to determine the ultimate load capacity; the sampling ratio is 1%. Destructive testing should be used for important structural members, cantilevered structures, or where there is doubt about anchoring quality.
Q6Which certifications related to on-site testing have Daring back bolts passed?
The Daring back-bolt system has fully passed Tongji University's grade-9 rare-earthquake seismic test (acceleration 1.24g), and a 2023 test report has been issued. The back bolts are made of 304/316 stainless steel and have passed a 2-million-cycle fatigue test, a 120-minute fire resistance test and salt spray testing. Daring can provide material analysis reports, load capacity reports and seismic test reports.

The Daring back-bolt range covers hammer-in, screw-in and cast-in back bolts as well as high-load back bolts, all made of 304/316 stainless steel and supported by dedicated drilling machines, hole-gauge rods, hole gauges and other inspection tools. The Daring back-bolt dry-hung cladding system has fully passed Tongji University's grade-9 rare-earthquake seismic test, with acceleration reaching 1.24g; back bolts, undercut anchors and Anka anchors have all obtained EU ETA certification. For guidance on designing on-site back-bolt inspection schemes and selecting inspection tools for specific projects, please consult the Daring technical team.

References

JGJ 133-2001, Technical Code for the Engineering of Metal and Stone Curtain Walls — structural requirements for back-bolt support connections

JGJ 336-2016, Technical Code for the Engineering of Man-Made Panel Curtain Walls — back-bolt inspection requirements in clauses 10.2.6 and 10.2.7

JGJ 145-2013, Technical Specification for Post-Installed Anchorage in Concrete Structures — Appendix C: on-site inspection methods and evaluation criteria for anchorage load capacity

GB 50210, Code for Acceptance of Quality of Building Decoration — main-control items for acceptance of curtain-wall works

Daring website — What on-site inspections are required after curtain-wall back-bolt installation? A full analysis of inspection items and standards

Daring website — What should be done if a back-bolt pull-out test fails? A complete review of common causes and remedial measures

Daring website — Pull-out failure caused by substandard reaming at the bottom of curtain-wall back-bolt holes | Daring solutions and inspection tools explained