Chemical Anchors: The chemical anchor articles I wrote previously were all compiled based on existing experience, but some inquirers have only a superficial understanding of chemical anchors themselves, so such articles are not of much help to them. Now I want to start with the most basic things, so that anyone who reads the article can gain a comprehensive and systematic understanding of chemical anchors.

Standard Chemical Anchor Models

Earlier I wroteClassification and Uses of Chemical AnchorsWe learned that chemical anchors are divided into three types: high-strength chemical anchors, reverse-cone anchors, and capsule anchors. This time we will give a comprehensive explanation of the specifications and models of chemical anchors. Although no relevant standard defines their specifications and models, industry insiders have basically established a distinction between national-standard and non-standard. The national-standard models of the three types of chemical anchors are basically the same, and their specifications are as follows:

Table 1. Chemical Anchor Specifications and Technical Parameters

Product Model

Drilling Diameter

Drilling Depth

Maximum Anchoring Thickness

Minimum Base Material Thickness

Total Threaded Rod Length

Remarks

M8×110

10

80

15

120

110

High-Strength Chemical Anchor Model

M10×130

12

90

20

130

130

General Model

M12×160

14

110

25

160

160

M16×190

18

125

35

175

190

M20×260

25

170

65

220

260

M24×300

28

210

65

270

300

M30×380

35

280

70

340

380

Table 1 shows the conventional specifications of chemical anchors. Most manufacturers do not produce M8 reverse-cone anchors or capsule anchors; of course, the usage of M8 chemical anchors is itself very small.

Customization of Non-Standard Chemical Anchors

Speaking of national standards leads to non-standard ones. Currently, non-standard specifications mainly arise in the following two situations:

1) Increasing the exposed length of the threaded rod. This approach is due to the anchored object being relatively thick; provided the anchor's own tensile and shear mechanical properties are satisfied, such an approach is acceptable. Such extended-length chemical anchors require special customization, and the processing cycle is considerably longer than for standard models. Only with a moderate quantity (over ten thousand) can one negotiate better pricing and follow-up service with the chemical anchor manufacturer.

2) Increasing the embedment depth. This approach is not a good one and requires further verification. Taking a grade 5.8 M12 chemical anchor as an example, the national-standard embedment depth is 110 mm, and the pull-out test result in C30 concrete is rupture of the anchor itself, which indicates that an embedment depth of 110 mm is already fully sufficient to develop the ultimate mechanical properties of the anchor material (35# steel). A greater embedment depth has no practical significance and may even increase construction difficulty, bringing nothing but disadvantages. This is a misconception among many designers: they do not understand where the limit of anchor load capacity lies, and blindly increasing the anchor length only makes construction more difficult and raises project costs. Taking another example, a grade 5.8 M24 chemical anchor with a national-standard embedment depth of 210 mm, when installed with a chemical cartridge, gives a pull-out test result in C30 concrete of failure at the concrete-adhesive interface. In this case, increasing the embedment depth and lengthening the chemical cartridge (with a corresponding increase in adhesive volume) will correspondingly increase the mechanical performance. However, if the original mechanical performance already meets the project's needs, the added performance is of little use, and it is difficult to find a manufacturer willing to produce extra-long large-size chemical cartridges on the market, making the project hard to proceed. We can only adopt another approach: use injection anchoring adhesive during installation. Once the adhesive has fully developed its strength, the threaded rod will rupture at the standard embedment depth — this is the simplest method of improvement. Simply put, for small-size (M16 and below) chemical anchors there is no need at all to increase the embedment depth; forcing an increase only adds cost and workload. For large-size (M20 and above) chemical anchors, injection anchoring adhesive can be used during installation, and there is likewise no need to increase the embedment depth.

Daring has supplied chemical anchors up to M56×1500 for nuclear power projects and has extensive service experience; you can consult Daring about relevant customization solutions. However, I have encountered several customers inquiring about M14 and M27 chemical anchors. These are actually special specifications created by certain manufacturers to be different; Daring does not produce or customize these two specifications.